压力容器2001,Vol.18Issue(3):19-22,4.
钢制轻烃球罐多发性裂纹性质及成因研究
Investigation on Character and Cause of Regular Cracks for Steel Light-Hydrocarbon Spherical Tanks
郑启文 1郑本和 1张清棠 2周亚春3
作者信息
- 1. 哈尔滨焊接研究所
- 2. 吉林化学工业股份有限公司
- 3. 大庆石油化工总厂
- 折叠
摘要
Abstract
Situation,type,character,affected factors,cause and mechanism of regular cracks for steel light-hydrocarbon spherical tanks in Daqing and Jilin zone were studied.The results showed that the higher H2S content in active medium,brittle-hard gross-grain martensite strcture in welded zone,larger welding residual stress,segregation of S and P etc.impurity in shell material were main cause for above cracks.关键词
钢制轻烃球罐 H2S应力腐蚀裂纹(SSCC)分类
机械制造引用本文复制引用
郑启文,郑本和,张清棠,周亚春..钢制轻烃球罐多发性裂纹性质及成因研究[J].压力容器,2001,18(3):19-22,4.