四川大学学报(自然科学版)2004,Vol.41Issue(2):373-378,6.
硅铁阳极溶出非隔膜电解制备高铁酸钠
Electrochemical Preparation of Sodium Ferrate(Ⅵ) Using Silicon Iron as Anode in Non-Diaphragm Electrobath
刘永春 1谢家理2
作者信息
- 1. 乐山师范学院环境与生命科学系,四川,乐山,614000
- 2. 四川大学化学学院,成都,610064
- 折叠
摘要
Abstract
Using silicon iron as anode to preparation sodium ferrate(Ⅵ) in non-diaphragm electrobath. The maximum current yield was reached to 43.0% (concentration of ferrate (Ⅵ) is electrolysis duration is 180mins. It proved that silicon iron anode is better than other reported anode, such as carbon iron or zinc white ironanode ect..关键词
高铁酸钠/非隔膜电解/硅铁/电流效率Key words
sodium ferrate/non-diaphragm electrolysis/silicon iron/current efficiency分类
化学化工引用本文复制引用
刘永春,谢家理..硅铁阳极溶出非隔膜电解制备高铁酸钠[J].四川大学学报(自然科学版),2004,41(2):373-378,6.