燃料化学学报2005,Vol.33Issue(5):590-596,7.
还原温度与时间对铁基催化剂浆态床F-T合成性能的影响
Effect of reduction temperature and duration on iron-based catalyst for slurry phase Fischer-Tropsch synthesis
摘要
Abstract
The Fischer-Tropsch synthesis (FTS) over a spray-dried iron-based catalyst reduced at different conditions was investigated in a continuous stirred tank reactor. The effects of reduction temperature and duration on the FTS performances as well as bulk compositions and other properties of the catalyst were determined. The results indicate that the extent of reduction and carburization was intensified by prolonging the reduction duration or by increasing the reduction temperature. The catalyst activity and stability was enhanced with the reduction at 270 ℃ compared with those reduced at lower temperature (240 ℃) or unreduced samples. The working catalyst loss during FTS resulted in the catalyst rapid deactivation at lower reduction temperature. The product distribution shifted towards lower molecular weight hydrocarbons with increasing reduction temperature or prolonging reduction duration at the same temperature.关键词
F-T合成/还原温度/还原时间/浆态床反应器/铁基催化剂/喷雾干燥Key words
Fischer-Tropsch synthesis/reduction temperature/reduction duration/slurry reactor/iron-based catalyst/spray-drying technology分类
化学化工引用本文复制引用
郝庆兰,白亮,郝栩,相宏伟,李永旺,易凡,徐斌富..还原温度与时间对铁基催化剂浆态床F-T合成性能的影响[J].燃料化学学报,2005,33(5):590-596,7.基金项目
国家自然科学基金 (20590361) (20590361)
国家高技术研究发展计划 (2001AA523010) (2001AA523010)
中国科学院知识创新重大项目 (KGCX1-SW-02).National Natural Science Foundation of China (20590361) (KGCX1-SW-02)
National High-Tech Research and Development Program of China (863 Program, 2001AA523010) (863 Program, 2001AA523010)
Key Engineering Project of Chinese Academy of Sciences (KGCX1-SW-02). (KGCX1-SW-02)