| 注册
首页|期刊导航|理化检验-物理分册|Q460C钢板力学性能不合格原因分析

Q460C钢板力学性能不合格原因分析

孙胜英 张志杰 靳芳芳 张海旺

理化检验-物理分册2011,Vol.47Issue(2):120-122,3.
理化检验-物理分册2011,Vol.47Issue(2):120-122,3.

Q460C钢板力学性能不合格原因分析

Cause Analysis of Unqualified Mechanical Properties of Q460C Steel Plates

孙胜英 1张志杰 1靳芳芳 1张海旺1

作者信息

  • 1. 邯郸钢铁集团有限责任公司技术中心,邯郸,056015
  • 折叠

摘要

Abstract

Reasons of mechanical properties of multiple batches of Q460C steel plates produced by a steel plant lower than the requirement of GB/T 1591 - 2008 were analyzed through optical microscope and scanning electron microscope.The results show that the bainite structure, tiny cracks and MnS inclusions as well as Nb and Ti compound inclusions caused by center segregation were the main reasons for the unqualified mechanical properties of Q460C steel plates.And widmanstatten structure caused by improper rolling technics also lowered the mechanical properties of the Q460C steel plates.

关键词

Q460C钢板/力学性能/贝氏体组织/魏氏组织/夹杂物/微裂纹

Key words

Q460C steel plate/ mechanical property/ bainite structure/ widmanstatten structure/ inclusion/tiny crack

分类

矿业与冶金

引用本文复制引用

孙胜英,张志杰,靳芳芳,张海旺..Q460C钢板力学性能不合格原因分析[J].理化检验-物理分册,2011,47(2):120-122,3.