航空材料学报2009,Vol.29Issue(6):107-112,6.DOI:10.3969/j.issn.1005-5053.2009.6.022
航空有机玻璃紫外光老化研究
Study on Accelerated Ageing of Aeronautical Perspex(PMMA) in Ultraviolet
陈新文 1裴高林 1金玉顺2
作者信息
- 1. 北京航空材料研究院,北京,100095
- 2. 北京石油化工学院,北京,102617
- 折叠
摘要
Abstract
The accelerated ageing experiment of Perspex (PMMA) YB-DM-11 were done for nearly two months in both 254nm and 313nm wave length ultraviolet. Tensile stress and mass were measured during the experiment. Thus the changing rules of both parameters were obtained. The samples structure difference were founded between before ageing and after ageing by methods of IR, TG/DTA,GPC and SEM. Analyzed results above all, the ageing mechanisms of PMMA in ultraviolet were clarified qualitatively.关键词
有机玻璃/紫外光/加速老化/老化规律/老化机理Key words
perspex(PMMA)/ultraviolet/accelerated ageing/ageing rule/aging mechanism引用本文复制引用
陈新文,裴高林,金玉顺..航空有机玻璃紫外光老化研究[J].航空材料学报,2009,29(6):107-112,6.