丝绸2011,Vol.48Issue(7):8-10,14,4.
改性涤纶织带阳离子染料轧染染色
Pad dyeing of modified polyester ribbon with cationic dyes
姜志新 1宋金龙 1张原岽1
作者信息
- 1. 浙江三鼎织造有限公司,浙江,义乌,322000
- 折叠
摘要
Abstract
In view of higher energy consumption of polyester ribbon with disperse dyes with conventional thermosol dyeing, the effects of dyeing temperature, fixation time, pH value of dyeing bath and dosage of leveler PE for dyeing behaviors of modified polyester ribbon with cationic dyes in low temperature pad dyeing were discussed. The results showed that modified polyester ribbon could obtain good color evenness and fastness when dyeing temperature under 100 ℃, fixation time 2.5 min, pH value of dyeing bath 4, and leveler PE 20 g/L. Compared with conventional thermosol dyeing, pad dyeing of modified polyester ribbon could save the comprehensive consumption of water and energy. Meanwhile, a large amount of waste water disposal can be decreased.关键词
阳离子染料/改性涤纶/轧染/染色性能Key words
Cationic dye/ Modified polyester/ Pad dyeing/ Dyeing property分类
轻工纺织引用本文复制引用
姜志新,宋金龙,张原岽..改性涤纶织带阳离子染料轧染染色[J].丝绸,2011,48(7):8-10,14,4.