Abstract

Preparation of high-purity antimony oxychloride from high-arsenic refined bismuth dust in a process of hydrochloric acid leaching, antimony powder reduction, hydrolysis, hydrochloric acid dissolution, impurity removal, hydrolysis was studied. In the process of leaching with hydrochloric acid, the leaching rates of Sb, As, Bi and Pb are 99.50%, 92.79%, 95.12% and 85.34% when the ratio of hydrochloric acid solutions to refined bismuth dust is 3:1, reaction time is 4 h, reaction temperature is 80 V, the content of hydrochloric acid is 1.2 times of its theoretical content. Sb5+ is reduced to Sb3+by adding antimony powder into the hydrochloric acid leaching solution, which is then hydrolyzed. The hydrolysis rate of Sb3+ arrives at 98.25% when the reaction temperature is 20 ℃, reaction time is 1 h, and the ratio of water to SbCl3 solution is 10:1. After the hydrolysate is dissolved by hydrochloric acid solutions and the impurity is removed after 1 h by means of adding agent, the solution is hydrolyzed and the products is obtained by means of filtration, washing and drying. The content of Sb in the products arrives at 75.71% and the impurity contents of As, Pb, Bi are 0.081 9%, 0.039 2% and 0.118 7%, respectively. The product is rhombohedral particles with the advantages of uniform size and its chemical formula is Sb4O5Cl2.

关键词

精炼铋烟尘/盐酸浸出/除杂/氯氧化锑

Key words

refined bismuth dust/ hydrochloric acid leaching/ removing impurities/ antimony oxychloride

分类

矿业与冶金

引用本文复制引用

郑雅杰,滕浩,白猛..以高砷精炼铋烟尘为原料制备高纯氯氧化锑[J].中南大学学报(自然科学版),2011,42(6):1549-1554,6.

基金项目

广东省教育部产学研重大项目(2008A090300016) (2008A090300016)

中南大学学报(自然科学版)

OA北大核心CSCDCSTPCD

1672-7207

访问量0
|
下载量0
段落导航相关论文