强激光与粒子束2011,Vol.23Issue(6):1559-1563,5.DOI:10.3788/HPLPB20112306.1559
溶胶-凝胶法制备W-Ir混合金属基阴极
Preparation of W-Ir mixed metal-based cathode by Sol-Gel method
摘要
Abstract
Because the general mixed metal matrix cathode can't meet emission performance needs, the research focus on the W-Ir mixed metal-based cathode made with Sol-Gel method. The composition, microgram and granularity of the power and the surface and inner of the mixed metal-based cathode are studied by XRD and SEM. The emission performance of the mixed metal-based cathode has been measured. And the influence of activation temperature and time on the emission performance has been studied. The results show that the surface and inner structure and the emission performance of the mixed metal-based cathode made with Sol-Gel method are all better than the general mixed metal matrix cathode made with solid-liquid doping.关键词
溶胶凝胶法/混合金属基阴极/发射性能/发射电流密度/图像分析Key words
Sol-Gel/mixed metal-based cathode/emission performance/current density/imaging analysis分类
数理科学引用本文复制引用
王传璟,陈怀璧,王燕春..溶胶-凝胶法制备W-Ir混合金属基阴极[J].强激光与粒子束,2011,23(6):1559-1563,5.基金项目
国家自然科学基金项目(10775080) (10775080)