Under the same test conditions,cold cracking susceptibility and reheat cracking susceptibility of B610CF-L2 and JFE-HITEN610U2L steel alloy has been investigated by the maximum hardness,Y-groove test method and implant test in weld heat affected zone.Welding linear energy, related mechanics performance test and series of temperature impact test of welding joints is introduced, and toughness -brittleness transition temperature is also identified.Results show that the steel alloys have the same low cold cracking susceptibility and certain extent reheat cracking susceptibility,and former's reheat cracking susceptibility is lower than the latter.lt also illustrates that the ranges of welding linear energy are all wide,the mechanical properties of welding joints are at the same level, they are all of high quality in low temperature toughness with Akv2≥47J at -50 ℃ and their toughness-brittleness transformation temperature vTt.vTs<-50℃.They are adapted to -50℃ 2 000 m3 cryogenic ethylene spherical tank.

关键词

冷裂纹敏感性/再热裂纹敏感性/低温韧性

Key words

cold cracking susceptibility/reheat cracking susceptibility/low temperature toughness

分类

矿业与冶金

引用本文复制引用

张一任,何前进,房务农,陈前银..B610CF-L2与JFE一HITEN610U2L钢焊接性能对比研究[J].电焊机,2012,42(2):74-78,5.

电焊机

OA北大核心CSTPCD

1001-2303

访问量0
|
下载量0
段落导航相关论文