摘要

Abstract

Three industrial 7-Al2O3s, namely W203, W217 and W251, were used as supports of Pd/γ-Al2O3 catalysts, in which W203 and W217 were typical mesoporous 7-Al2 O3 supports, and W251 was a special macroporous support. Catalytic activity of the Pd/γ-Al2 O3 catalysts in hydrogenation of C9 petroleum resin was investigated. The 7-Al2O3 supports and the Pd/γ-Al2O3 catalysts were characterized by means of N2 adsorption-desorption, CO chemisorption, SEM, TEM and XRD. The results indicated that the influence of the pore structure of the supported catalysts on the catalytic hydrogenation of C9 petroleum resin was significant and the catalyst with adequate macroporous structure showed higher activity and stability in catalytic hydrogenation of the macromolecules. Average pore sizes of the three industrial -y-Al2O3s, and activity and stability of the Pd/7-Al2O3 catalysts followed with the same order: W203 < W217 < W251. Pd precursor could easily enter into W251 support interior with macropores, so the Pd dispersion was promoted and the catalyst with "egg white" structure formed.

关键词

碳九石油树脂/γ-氧化铝载体/催化加氢/钯催化剂

Key words

C9 petroleum resin/γ-alumina support/catalytic hydrogenation/palladium catalyst

分类

化学化工

引用本文复制引用

鲁佳,马磊,江大好,卢春山,张群峰,李小年..γ - Al2O3载体孑结构对负载钯催化剂催化C9石油树脂加氢性能的影响[J].石油化工,2011,40(10):1105-1109,5.

石油化工

OA北大核心CSCDCSTPCD

1000-8144

访问量0
|
下载量0
段落导航相关论文