| 注册
首页|期刊导航|烟草科技|卷烟热塌陷的测试方法

卷烟热塌陷的测试方法

宋旭艳 张华 李文璟 罗诚浩 魏敏

烟草科技Issue(1):5-9,5.
烟草科技Issue(1):5-9,5.

卷烟热塌陷的测试方法

Method for Measuring Hot Collapse of Cigarette

宋旭艳 1张华 1李文璟 1罗诚浩 1魏敏1

作者信息

  • 1. 湖北中烟工业有限责任公司,武汉市汉阳区十升路22号 430051
  • 折叠

摘要

Abstract

For accurately measuring the hot collapse of cigarette during smoking, a method for measuring the hot collapse of tobacco rod and filter plug of cigarette with smoking machine was established by optimizing the method recommended by CORESTA. The optimized testing conditions were: l)the sample amount for tobacco rod test was 10, butt length was tipping paper length +10 mm, the test position should be on tipping paper length + 3 mm measured from the mouth end; 2)the sample amount for filter tip test was 5,butt length was tipping paper length +3 mm, and the test position should be on filter plug length minus 5 mm measured from the mouth end; under which the RSD was under 10%. The method was suitable for test batches of samples.

关键词

卷烟/滤嘴/热塌陷/单孔道吸烟机

Key words

Cigarette/Filter/Hot collapse/Single port smoking machine

分类

轻工纺织

引用本文复制引用

宋旭艳,张华,李文璟,罗诚浩,魏敏..卷烟热塌陷的测试方法[J].烟草科技,2012,(1):5-9,5.

基金项目

烟草行业推荐性标准制、修订项目"卷烟和滤棒物理性能的测定-热塌陷"(2007B007). (2007B007)