| 注册
首页|期刊导航|理化检验:物理分册|超超临界机组T92钢高温受热面管爆管原因分析

超超临界机组T92钢高温受热面管爆管原因分析

赵彦芬 张路 刘艳 许万军

理化检验:物理分册2012,Vol.48Issue(3):180-184,5.
理化检验:物理分册2012,Vol.48Issue(3):180-184,5.

超超临界机组T92钢高温受热面管爆管原因分析

Reason Analysis on Bursting Tube of High Temperature Boiler Tube of T92 Steel in Ultra Supercritical Unit

赵彦芬 1张路 1刘艳 1许万军2

作者信息

  • 1. 苏州热工研究院有限公司,苏州215004
  • 2. 华电国际芜湖发电有限公司,芜湖241000
  • 折叠

摘要

Abstract

The platen superheater tube failures of T92 steel has bursted in a ultra supercritical power plants. The bursting reason was analyzed by means of macroscopical inspection, chemical composition analysis, hardness testing, tensile strength testing, metallographie examination and so on. Results showed that the microstructure of the tube which didn't maintenance the typical lath martensite, the phase transformation at Ac~ ~Aca after short- term overheated. The strength decreased rapid distinctly, therefore the strength was not enough to endure the stress, finally the tube bursted. On the other hand, the relationship between the different microstructure and mechanical property was achieved by test in order to supervise for metal in thermal power plants for long term operation.

关键词

T92钢/超超临界机组/爆管/强度/应力

Key words

T92 steel/ultra supercritical unit/bursting tube/strength~ stress