| 注册
首页|期刊导航|陶瓷|高透光细瓷的制备

高透光细瓷的制备

包启富 董伟霞 陈望强

陶瓷Issue(3):22-25,4.
陶瓷Issue(3):22-25,4.

高透光细瓷的制备

Preparation of Porcelain with the High Transmission Efficiency

包启富 1董伟霞 1陈望强1

作者信息

  • 1. 景德镇陶瓷学院 江西景德镇333001
  • 折叠

摘要

Abstract

In this study,green body was prepared by lithium porcelain stone,quartz, Longyan kaolin.feldspar.talc as the main raw ma-terial, sodium bentonite and humic acid adjusting the molding performance The high mechanical strength and light transmission were studied by the simple factor and orthogonal test. When the lithium-China Stone 40, quartz 27, Longyan Kaolin 32, K-feldspar 8, burning talc 1. 5, bentonite 2,frit 2,humic acid sodium 0. 8,alumina 2, the porcelain with high light trans mission were sintered at I 320 ℃ at reducing atmosphere. The porcelain's transmission is up to 27. 5.

关键词

细瓷/透光度/抗折强度

Key words

Porcelain/ Tratismittance efficiency/ Flexstrength

分类

化学化工

引用本文复制引用

包启富,董伟霞,陈望强..高透光细瓷的制备[J].陶瓷,2012,(3):22-25,4.