焊管2012,Vol.35Issue(6):9-12,4.
X100管线钢埋弧焊用烧结焊剂的研制
Development of Sintered Flux Used for X1O0 Pipeline Steel Submerged-arc Welding
张敏 1陈飞绸 1李继红1
作者信息
- 1. 西安理工大学材料科学与工程学院,西安710048
- 折叠
摘要
Abstract
In this article, it introduced slag system selection of flux used for X100 pipeline steel submerged-arc welding, alkalinity range determination, as well as analysis on welding process and mechanical performance Using H03MnNi3MoTiB wire which is matched with X100 to conduct double wire submerged-arc welding test, the results indicated that the quality of weld and HAZ both meet the requirements of API SPEC 5L , but some black spot exist in bead surface. The composition of black spot is iron oxide by energy spectrum analysis, a kind of improved approach of removing black spot, increasing slag protection and reducing the content of oxygen in weld, is proposed, so the prescription for excellent flux to X100 pipeline steel has been obtained.关键词
X100管线钢/烧结焊剂/冲击韧性Key words
X100 pipeline steel/ sintered flux/ impact toughness
分类
矿业与冶金引用本文复制引用
张敏,陈飞绸,李继红..X100管线钢埋弧焊用烧结焊剂的研制[J].焊管,2012,35(6):9-12,4.