In practical manufacture, we found that welding rod of the same trademark but different batch has distinct different tendency of brittleness when they are experienced step cooling embrittling treatment process. The chemical composition,mechanical properties,ductile -brittle transition temperature and metallurgical microscope of 2.25Cr- 1 Mo -0.25 V steel have been investigated,and the results show that the reason of temper brittleness is that the content of Si and Mn are high and phosphorus and carbonization segregation on grain boundary.关键词
2.25Cr-1Mo-0.25V焊缝/回火脆性/显微组织Key words
2.25Cr -1 Mo -0.25V steel/temper brittleness/microstructure分类
机械制造引用本文复制引用