Abstract

Causes and preventing measures of yarn long thin places defect were discussed. Classification and characteristics of yarn long thin places defect were introduced. The causes were analyzed and related modified measures were put forward. It is considered that some problems should be solved as key,such as missing sliver in finish doubling,roving and sliver worse package,worse switch machine,higher doubling speed,too much sliver drawing,rubber-covered roll and apron winding fiber,worse draft gear meshing,worse guiding sliver tension and spinning suspended status et al. Defect existed in autoleveler device embossing roller sensor should be eliminated. Autoleveler delay time should be set correctly, width and pressure of embossing roller should be selected properly. Absolute measurement electronic yarn cleaner was adopted,finally better prevent effect can be made.

关键词

长细节纱疵/缺条/开关车/牵伸齿轮/吊锭/自调匀整

Key words

Long Thin Places Defect/Missing Sliver/Switch Machine/Draft Gear/Suspended Spindle/Autoleveler

分类

轻工纺织

引用本文复制引用

戚建萍,刘荣清..细纱长细节纱疵的形成原因与防治措施[J].棉纺织技术,2012,40(10):48-51,4.

棉纺织技术

OA北大核心

1001-7415

访问量0
|
下载量0
段落导航相关论文