| 注册
首页|期刊导航|表面技术|四种典型牺牲阳极在干湿交替环境中的性能评价

四种典型牺牲阳极在干湿交替环境中的性能评价

方志刚

表面技术2012,Vol.41Issue(4):31-34,4.
表面技术2012,Vol.41Issue(4):31-34,4.

四种典型牺牲阳极在干湿交替环境中的性能评价

Performance Evaluation of Four Typical Sacrificial Anodes under Wet-dry Cyclic Environment

方志刚1

作者信息

  • 1. 海军装备研究院,北京100161
  • 折叠

摘要

Abstract

The change regulations of working potentials, electric currents, morphology and compositions of dissolved products for four typical sacrificial anodes were investigated in simulated seawater and simulated marine atmospheric environment for wet-dry cycles. The results showed that the performance of the four anodes under wet-dry cyclic environment decreased in the following order: Al-Zn-In-Mg-Ga-Mn anode, Al-Zn-In-Mg-Ti anode, Al-Zn-In-Cd anode, Zn-Al-Cd anode. Hence Al-Zn-In-Mg-Ga-Mn alloy with appropriate composition was an ideal anode material under wet-dry cyclic environment.

关键词

牺牲阳极/干湿交替/防腐蚀/评价

Key words

sacrificial anode/ wet-dry cycle/ anti-corrosion/ evaluation

分类

矿业与冶金

引用本文复制引用

方志刚..四种典型牺牲阳极在干湿交替环境中的性能评价[J].表面技术,2012,41(4):31-34,4.