The source of yak tail hair is plentiful in our country, but this kind of fiber can mainly be used in woolen fabric field due to its coarseness and stiffness. In this research yak tail hair are pretreated, stretched, setted and repaired with transglutaminase (TG) to improve the practical performance and added value. The results show that the optimum effect is obtained when pH is 7.0, temperature 70 ℃., treating time 60 min, and the MEate concentration 30 g/L. During stretching-setting process twisting on yak tail hair strend can enhance the fibers' luster. When TG is 2%(owf) the best repairing effect of tensile is gotten.关键词