锦屏一级水电站拱坝混凝土碱骨料反应抑制工程措施
Engineering measures for inhibiting concrete alkali-aggregate response during construction of high arch dam of Jinping Ⅰ Hydropower Station
李光伟 1周麒雯1
作者信息
- 1. 中国水电顾问集团成都勘测设计研究院,四川成都610071
- 折叠
摘要
Abstract
As limited by the objective circumstances, the metamorphosed quartz sandstone with potential alkali reactivity has to be adopted to the artificial aggregate for the concrete of the arch dam for Jinping I Hydropower Station. In accordance with the results from the testing made on the actual measures for the inhabitation of the concrete alkali-aggregate response, it is indicated that the expansive deformation from the alkali-aggregate response of the metamorphosed quartz sandstone in the concrete can be effectively inhibited by the engineering measures such as composited aggregate, mixing with high fly ash content of 35% , control of total alkali content, etc. .关键词
混凝土/碱骨料反应/抑制措施/组合骨料/混凝土总碱含量/高拱坝/锦屏一级水电站Key words
concrete/ alkali aggregate response/ inhibition measures/ combined aggregate/ total alkali content in concrete/ high arch dam/ Jinping I Hydropower Station分类
建筑与水利引用本文复制引用
李光伟,周麒雯..锦屏一级水电站拱坝混凝土碱骨料反应抑制工程措施[J].水利水电技术,2013,44(1):45-49,5.