| 注册
首页|期刊导航|湿法冶金|降低湿法炼锌中性浸出液中锗浓度的试验研究

降低湿法炼锌中性浸出液中锗浓度的试验研究

陈科彤 汤顺贤 刘贤

湿法冶金Issue(2):136-138,3.
湿法冶金Issue(2):136-138,3.DOI:10.13355/j.cnki.sfyj.2014.02.17

降低湿法炼锌中性浸出液中锗浓度的试验研究

Removal of Germanium From Neutral Leaching Solution During Zinc Hydrometallurgy

陈科彤 1汤顺贤 2刘贤2

作者信息

  • 1. 昆明冶金研究院,云南昆明 650031
  • 2. 云南驰宏锌锗股份有限公司,云南曲靖 655000
  • 折叠

摘要

Abstract

Removal of germanium from neutral leaching solution during zinc hydrometallurgy was researched .The effect of iron concentration ,pH of leaching end point ,leaching time and temperature , production flow and production continuity on the germanium concentration in neutral leaching solution were examined .The results show that under the conditions of iron mass concentration of 1 .57 g/L ,pH of leaching end point of 5 .0-5 .2 ,leaching temperature of 78-82 ℃ ,leaching time of 3-5 hours and flow of 140-160 m3/h ,germanium concentration can be controlled less than 0 .6 mg/L ,the leaching solution can meet .zinc electrowinning requirements .

关键词

湿法冶金//中性浸出//去除

Key words

zinc hydrometallurgy/neutral Leaching/germanium/removal

分类

矿业与冶金

引用本文复制引用

陈科彤,汤顺贤,刘贤..降低湿法炼锌中性浸出液中锗浓度的试验研究[J].湿法冶金,2014,(2):136-138,3.