表面技术Issue(4):164-167,4.
铸铝合金组合件阴极电泳涂装漆膜缩孔产生原因与解决方法
Causes and Solutions of Shrinkages of Cathodic Electrophoretic Coating Film on Cast Aluminum Alloy Assembly
王晓敦 1赵光煜2
作者信息
- 1. 淮海工业集团有限公司,山西 长治 046012
- 2. 西南技术工程研究中心,重庆 400039
- 折叠
摘要
Abstract
Objective To solve the problem of shrinkages of cathodic electrophoretic coating film on die-cast aluminum alloy as-sembly. Methods By analyzing the causes of shrinkages of cathodic electrophoretic coating film, parameters of tank liquor in skim-ming section, forming section and electrophoresis section were adjusted. The duration of skimming section was extended. After be-ing coated under 180 V voltages, the assembly was roasted and solidified. Results Upon inspection, the film on the assembly was flat and smooth and the shrinkage was eliminated. Salt spray resistance could up to 1000 h. The product acceptance requirements of the overall performance of the film were satisfied. Conclusion By adjusting the pretreatment process and the construction param-eters of electrophoresis coating, the shrinkages on the die-cast aluminum alloy assembly is eliminated and the antiseptic property of ammo is improved.关键词
铸铝合金组合件/电泳涂装/漆膜缩孔Key words
die-cast aluminum alloy assembly/electrophoresis coatings/shrinkages on the coating film分类
化学化工引用本文复制引用
王晓敦,赵光煜..铸铝合金组合件阴极电泳涂装漆膜缩孔产生原因与解决方法[J].表面技术,2014,(4):164-167,4.