火炸药学报Issue(6):53-57,5.DOI:10.14077/j.issn.1007-7812.2014.06.012
物理界面对炸药慢速烤燃特性的影响
Effect of Physical Interface on Slow Cook-off Characteristics of Explosives
高峰 1智小琦 1刘学柱 2牛新立3
作者信息
- 1. 中北大学地下目标毁伤技术国防重点学科实验室,山西 太原 030051
- 2. 山西江阳化工有限公司,山西 太原 030041
- 3. 黑龙江北方工具有限公司,黑龙江 牡丹江 157000
- 折叠
摘要
Abstract
A slow cook-off test of RDX based high energy explosives was conducted at a heating rate of 1℃/min by using self-designed cook-off test apparatus.Numerical simulation was performed using FLUENT software.The effects of three kinds of physical interface (air,T-09 and GPS-2 )on slow cook-off characteristics of explosives were researched.The results show that physical interface is an important factor affecting the slow cook-off response characteristics of explosive. Under the same conditions,air as physical interface can increase response temperature,response time and the response severity of the cook-off bomb.Inert material as physical interface can increase the response temperature,the response time of cook-off bomb and reduce the severity of the cook-off response.The numerical calculation results show that cook-off response to temperature and cook-off time are affected by the physical layer thickness of explosive.When the range of the physical layer thickness is 0-5 mm,cook-off response temperature and cook-off time increase with increasing the physical layer thickness.When physical layer thickness increases to 2.5mm,cook-off response temperature and cook-off time reach to maximum,then decrease with increasing the physical layer thickness.关键词
物理化学/物理界面/慢速烤燃试验/炸药/热爆炸/FLUENT软件Key words
physical chemistry/physical interface/slow cook-off test/explosive/thermal explosion/FLUENT software分类
军事科技引用本文复制引用
高峰,智小琦,刘学柱,牛新立..物理界面对炸药慢速烤燃特性的影响[J].火炸药学报,2014,(6):53-57,5.