| 注册
首页|期刊导航|临床口腔医学杂志|二硅酸锂和白榴石基玻璃陶瓷在模拟咀嚼循环下的耐磨性研究

二硅酸锂和白榴石基玻璃陶瓷在模拟咀嚼循环下的耐磨性研究

张珍珍 张少锋 郭嘉文 王琪 伊远平

临床口腔医学杂志Issue(1):9-11,12,4.
临床口腔医学杂志Issue(1):9-11,12,4.DOI:10.3969/j.issn.1003-1634.2015.01.004

二硅酸锂和白榴石基玻璃陶瓷在模拟咀嚼循环下的耐磨性研究

Abrasive resistance of lithium disilicate glass-ceramic and leucite reinforced glass-ceramic

张珍珍 1张少锋 1郭嘉文 1王琪 1伊远平1

作者信息

  • 1. 第四军医大学口腔医院修复科·军事口腔医学国家重点实验室 陕西 西安710032
  • 折叠

摘要

Abstract

Objective:To compare wear properties of leucite glass-ceramic and lithium disilicate glass-ceramic from the perspective of time-varying wear behavior. Method:Leucite reinforced glass-ceramic (IPS Empress Esthetic ETC1)and lithium disilicate glass-ceramic (IPS e.max Press HT) specimens were made by heat-pressed technology. The antagonist of steatite was subjected to the wear test method(a vertical force of 10N, one million cycles). The wear volume was mearsured by a three-dimensional profiler per 100,000 cycles,with SEM observing surface topography. Result:At 100,000 cycles vol-ume loss of leucite reinforced glass ceramic was more than lithium disilicate ceramic ,and there is no difference between the two ceramics after 200,000 cycles. At initial stage,leucite reinforced glass-ceramic showed the morphology of furrows and debris and lithium disilicate glass-ceramic demonstrated deep and wide furrows. With the evolution of time ,furrows of su-perficial and dense,the surface tends to be smooth. Conclusion:At initial stage,leucite reinforced glass-ceramic wore more than lithium disilicate glass-ceramic. However,there was no significant difference between the two heat-pressed glass ce-ramic at later stage.

关键词

牙瓷料/牙修复磨损/显微镜检查,电子,扫描

Key words

dental Porcelain/dental restoration wear/microscopy/electrochemical/scanning