Abstract
Amino-containing polyacrylate adhesive was prepared by emulsion polymerization technology, and the polymerization technology was optimized. The results showed that the dosage of initiator was 0.6%(on the total mass of monomers, the same below), the dosage of water-absorbing monomer acrylic acid was 3.5%, and the amount of acrylamide was 5%. The polymerization reaction temperature was 85 ℃, the holding time was 3.5 h.关键词
聚丙烯酸酯/丙烯酰胺/聚合工艺Key words
polyacrylate/acrylamide/polymerization分类