正己烷在成型无黏结剂5A分子筛上脱附特性研究

杜旭东 唐芸 崔群 王海燕 姚虎卿

高校化学工程学报Issue(1):32-37,6.
高校化学工程学报Issue(1):32-37,6.DOI:10.3969/j.issn.1003-9015.2013.01.006

正己烷在成型无黏结剂5A分子筛上脱附特性研究

Desorption Characteristic of n-Hexane Adsorbed on Binder-free 5A Zeolites

杜旭东 1唐芸 1崔群 1王海燕 1姚虎卿1

作者信息

  • 1. 南京工业大学 化学化工学院,江苏 南京 210009
  • 折叠

摘要

Abstract

The crystal structures of binder-free 5A zeolite pellets (5A-1, 5A-6) were determined by XRD, and the results show that the 5A-1 and 5A-6 zeolite pellets have strong XRD characteristic peaks of 5A zeolite and no other miscellaneous peak. The relative crystallinity of 5A-1 zeolite is 64% compared to that of the 5A-6 zeolite. The apparent desorption activation energy and desorption parameters of n-hexane adsorbed on binder-free 5A zeolite pellets were studied by thermo gravimetric differential analyzer (TG-DTA). The helium purging desorption curves of n-hexane adsorbed on 5A-1 and 5A-6 zeolite pellets were studied by a dynamic adsorption and desorption experimental equipment. The TG-DTA profiles of n-hexane adsorbed on 5A-1 and 5A-6 zeolite pellets show two desorption peaks:the activation energies of the first desorption peak on 5A-1 and 5A-6 zeolite pellets are 33.44 kJ⋅mol−1and 39.35 kJ⋅mol−1, respectively, while the activation energies of the second desorption peak are 52.21 kJ⋅mol−1 and 67.48 kJ⋅mol−1, respectively. The suitable desorption temperatures of n-hexane adsorbed on 5A-1 and 5A-6 zeolite pellets all exceed 200℃. The n-hexane adsorbed on 5A-1 and 5A-6 zeolite pellets can completely desorbed by being purged with helium at 200℃, and the 5A-1 zeolite pellet has better desorption performance than that of 5A-6.

关键词

正己烷/成型无黏结剂5A分子筛/脱附活化能/氦气/吹扫

Key words

n-hexane/binder-free 5A zeolite/desorption activation energy/helium/sweep

分类

化学化工

引用本文复制引用

杜旭东,唐芸,崔群,王海燕,姚虎卿..正己烷在成型无黏结剂5A分子筛上脱附特性研究[J].高校化学工程学报,2013,(1):32-37,6.

基金项目

国家自然科学基金(20876074) (20876074)

中石化项目(J106002) (J106002)

高校化学工程学报

OA北大核心CSCDCSTPCD

1003-9015

访问量0
|
下载量0
段落导航相关论文