| 注册
首页|期刊导航|焊管|HFW焊管热张力减径前后的压扁试验结果分析

HFW焊管热张力减径前后的压扁试验结果分析

窦茂科 陈浩明 吴涛 吴鹏飞 阎龙

焊管Issue(11):48-51,4.
焊管Issue(11):48-51,4.

HFW焊管热张力减径前后的压扁试验结果分析

Analysis on Flattening Test Result of HFW Pipe before and after Hot Stretch Reducing

窦茂科 1陈浩明 1吴涛 1吴鹏飞 1阎龙1

作者信息

  • 1. 宝鸡石油钢管有限责任公司,陕西 宝鸡 721008
  • 折叠

摘要

Abstract

Adopting a new process of high frequency welding(HFW)+hot stretch reducing (referred to as SEW)to conduct trial produce for oil casing billet,then the flattening tests were carried out respectively for sample pipe before and after hot stretch reducing. The results indicated that flattening tests all qualified, even if the sample is crushed to the lining joint, the specimens with tiny crack in weld are few. This showed that the plastic deformation capacity of weld is improved significantly, achieves the purpose of welded pipe seamless.

关键词

焊管/HFW管/SEW管/压扁试验/热张力减径

Key words

welded pipe/HFW pipe/SEW pipe/flattening test/hot stretch reducing

分类

矿业与冶金

引用本文复制引用

窦茂科,陈浩明,吴涛,吴鹏飞,阎龙..HFW焊管热张力减径前后的压扁试验结果分析[J].焊管,2015,(11):48-51,4.