某选厂尾矿回收铁的试验研究

路永森 王清林 黄立成

矿产保护与利用Issue(2):26-29,4.
矿产保护与利用Issue(2):26-29,4.

某选厂尾矿回收铁的试验研究

Experimental Research on Iron Recovery fromTailings of a Dressing Plant

路永森 1王清林 1黄立成1

作者信息

  • 1. 南钢集团冶山矿业有限公司,江苏南京,210000
  • 折叠

摘要

Abstract

The iron contained in the tailings of a dressing plant of an iron mine is 9 .30%, which has certain recovery value .In order to utilize the resource comprehensively , beneficiation tests were carried out .The tailings was treated first by pre -concentration with spiral chute , then the rougher concentrate was reground and went to a two -stage weak magnetic separation with a magnetic inten-sity of 20 KA/m.The open circuit test could output an iron concentrate containing 63.74% TFe with a recovery of 10 .09%.The iron ore has been recovered effectively by the process , and this will provide basis for the mine's subsequent technical reform .

关键词

尾矿/磁铁矿/预富集/磁选

Key words

tailings/magnetite/pre-concentration/magnetic separation

分类

矿业与冶金

引用本文复制引用

路永森,王清林,黄立成..某选厂尾矿回收铁的试验研究[J].矿产保护与利用,2013,(2):26-29,4.

矿产保护与利用

OACSTPCD

1001-0076

访问量0
|
下载量0
段落导航相关论文