In this paper,the ice crack glaze was prepared by using feldspar,dolomite,calcite,quartz and Longyan kaolin, etc as raw materials.Effect of firing temperature and processing condition on glaze crack was studied by single factor exper-iment.The experimental results show that:when the dipping glaze time and ball milling time are 30 s and 40 min,respec-tively,the glaze appears smooth and obvious ice crack effect,which is due to thermal expansion coefficient of 1×10-6/℃ at 1 250 ℃.

关键词

冰裂纹釉/热膨胀系数/烧成温度/工艺条件

Key words

Ice crack glaze/Thermal expansion coefficient/Firing temperature/Processing condition

分类

化学化工

引用本文复制引用

董伟霞,包启富,向文宝..仿龙泉哥窑冰裂纹釉工艺条件因素的研究∗[J].陶瓷,2016,(10):30-32,3.

基金项目

国家自然科学基金项目(项目编号:51562013)。 (项目编号:51562013)

陶瓷

1002-2872

访问量0
|
下载量0
段落导航相关论文