| 注册
首页|期刊导航|染整技术|纯仪纶纤维织物的染整加工

纯仪纶纤维织物的染整加工

尚润玲

染整技术Issue(10):17-19,25,4.
染整技术Issue(10):17-19,25,4.

纯仪纶纤维织物的染整加工

Dyeing and finishing of pure YILON fiber fabric

尚润玲1

作者信息

  • 1. 江阴职业技术学院,江苏江阴 214400
  • 折叠

摘要

Abstract

The dyeing and finishing of YILON fiber including pretreatment, dyeing and setting were introduced. Bleaching is the main process of pretreatment. Sodium chlorite bleaching was often adopted if finished fabric is white or sensitive color. No bleaching or hydrogen peroxide-acetic acid bleaching was applied if finished fabric with medium or dark shade. YILON fabric was dyed with a low energy level dye E, medium energy level dye SE or high energy level disperses dye S. The dyeing under normal pressure at 98~100 ℃ can be used if finished fabric is shallow or neutral color. The dyeing was at 110~120 ℃ if finished fabric was in deep color and higher color fastness was demanded. The thermal setting temperature of the finishing should be controlled under 175 ℃. Color fastness of the finished fabric can be achieved 4~5 level and pilling resistance can be reached 4 grade. The pH value on fabric surface well satisfies the requirement of products.

关键词

漂白/染色/定型/仪纶

Key words

bleaching/dyeing/finishing/YILON fabric

分类

轻工纺织

引用本文复制引用

尚润玲..纯仪纶纤维织物的染整加工[J].染整技术,2016,(10):17-19,25,4.

染整技术

OA北大核心

1005-9350

访问量0
|
下载量0