重型机械Issue(2):84-87,4.
节能型不锈钢冶炼工艺设计
Design for energy saving stainless steel refining process
王永1
作者信息
- 1. 中冶东方工程技术有限公司秦皇岛研究设计院,河北 秦皇岛 066004
- 折叠
摘要
Abstract
In recent years,the increment of stainless steel production capacity has exceeded incremental demand,and overcapacity will become more serious.Steelmaking plants have to run in a high effective and energy saving way.An energy saving stainless steel refining process from ore to billet has been developed.The process use nickel laterite ore and fine chrome ore as raw materials to produce molten nickel iron and chrome iron,these two molten iron hot charges to AOD furnace to produce stainless steel can substantially reduce the production cost.关键词
红土镍矿/铬粉矿/矿热炉/不锈钢Key words
nickel laterite ore/fine chrome ore/submerged arc furnace/stainless steel分类
矿业与冶金引用本文复制引用
王永..节能型不锈钢冶炼工艺设计[J].重型机械,2017,(2):84-87,4.