广东电力2017,Vol.30Issue(5):114-118,5.DOI:10.3969/gddl/gddl2017/1705/170521.htm
输电线路复合绝缘子运行状态抽样检测试验
Sampling Inspection Experiment on Operating State of Transmission Line Composite Insulator
黄振 1许志海 2彭向阳 1王锐 1张英 3周华敏3
作者信息
- 1. 广东电网有限责任公司电力科学研究院,广东 广州 510080
- 2. 广东电网有限责任公司机巡作业中心,广东 广州 510160
- 3. 广东电网有限责任公司,广东 广州 510060
- 折叠
摘要
Abstract
In order to control the situation of operating performance change of the running composite insulator, this paper introduces development of sampling inspection on transmission line composite insulator in the last four years of Guangdong power grid, and systematic experimental inspection on its macroscopic performance including hydrophobicity inspection, mechanical failure load, sealing property test , water diffusion with sheath, and so on. Sampling inspection results indicate that mechanical property of the composite insulator and sealing property of its ends are stable but performance such as interface adhesion, hydrophobicity and electrical erosion resistance of the umbrella skirt is clearly aging. Aging of performance is related with operating years of the composite insulator, performance of interface adhesion and electrical erosion resistance of the umbrella decreases obviously after the insulator operating over 8 years. In addition, declination of interface adhesion may cause declination of mechanical property of the core rod and even cause breakage fault, which should be closely paid attention to in operation and maintenance process.关键词
复合绝缘子/老化/抽检/界面粘接性/憎水性/运行年限Key words
composite insulator/aging/sampling inspection/interface adhesion/hydrophobicity/operating years分类
信息技术与安全科学引用本文复制引用
黄振,许志海,彭向阳,王锐,张英,周华敏..输电线路复合绝缘子运行状态抽样检测试验[J].广东电力,2017,30(5):114-118,5.