摘要

Abstract

The manufacturing of superalloy K465 component with special cavity via laser additive manufacturing was studied,in order to meet the design requirement of aerospace component with special cavity and ensure the mechanical properties at high temperature.The results indicated that the crack occurred during the additive manufacturing of superalloy K465 structure,because of the poor deformability and the existence of eutectic phase with low melting point,which made it to difficultly manufacture alone via laser additive manufacturing.By addingthe Stellite 6 alloy reasonably and reliefing the stress and heating the substance,the crack in the laser additive manufacturing significantly decreased.

关键词

激光增材制造/K465高温合金/裂纹/工艺控制

Key words

laser additive manufacturing/superalloy K465/crack/process control

分类

矿业与冶金

引用本文复制引用

施凡,赵吉宾,王志国,赵宇辉,姚超..K465合金激光增材制造加工工艺研究[J].机械科学与技术,2017,36(8):1298-1302,5.

基金项目

中科院重点部署项目(KGZD-EW-T04-2) (KGZD-EW-T04-2)

机械科学与技术

OA北大核心CSCDCSTPCD

1003-8728

访问量0
|
下载量0
段落导航相关论文