The aqueous suspension containing submicron-sized praseodymium-doped zirconium silicate as a ceramic yellow ink was prepared by wet ultrafine grinding in a stirred bead mill.The optimal technology parameters were investigated through an L34 orthogonal experiment with median diameter and uniformity coefficient of particle size distribution.The result shows that the optimal conditions include solid content of 30 wt%,bead loading of 80 vol%,stirrer tip velocity of 6.89m/s,grinding time of 1.25 h.

关键词

研磨参数/陶瓷墨水/正交试验/粒度分布

Key words

Grinding parameters/Ceramic inks/Orthogonal experiment/Particle size distribution

分类

化学化工

引用本文复制引用

蒙臻明,柯善军,祝乐民,梁立斌..正交试验优化镨黄陶瓷色料超细研磨工艺参数[J].陶瓷,2017,(5):28-31,4.

基金项目

广东省应用型科技研发专项(项目编号:2015B090927002) (项目编号:2015B090927002)

广东省产学研合作协同创新与平台环境建设项目(项目编号:2014B090903003). (项目编号:2014B090903003)

陶瓷

1002-2872

访问量0
|
下载量0
段落导航相关论文