| 注册
首页|期刊导航|陶瓷|黄兔毫釉的配方组成正交实验优化

黄兔毫釉的配方组成正交实验优化

董伟霞 包启富 李超

陶瓷Issue(11):33-36,4.
陶瓷Issue(11):33-36,4.

黄兔毫釉的配方组成正交实验优化

Orthogonal Experimental Optimization on the Formulation of the Yellow Hares Ful Glaze

董伟霞 1包启富 1李超1

作者信息

  • 1. 景德镇陶瓷大学材料与工程学院 江西景德镇333001
  • 折叠

摘要

Abstract

The formulation of hare's fur glaze were obtained by introducing Fe2O3 and TiO2 as crystal synthetics,and proper Ca3 (PO4)2 and boron frit as phase separation agent using orthogonal experimental method.The experiment showed that:its factors from large to small isrespectively silicon,boron frit,calcined talc,Fe2O3,TiO2,bone ash and kaolin.When the formulation is as follows:quartz 2.0%,boron frit 24.0%,calcinedtalc 4.0%,Fe2O3 6.0%,TiO2 1.0%,bone ash 1.5%,kaolin 7.0%,the finished hair's fur glaze shows a pale yellow and thin hails fur flow glaze at 1 280 ℃.

关键词

兔毫釉/配方组成/正交实验

Key words

Hare's ful glaze/Formulationorthogonal/Experimental method

分类

化学化工

引用本文复制引用

董伟霞,包启富,李超..黄兔毫釉的配方组成正交实验优化[J].陶瓷,2017,(11):33-36,4.

陶瓷

1002-2872

访问量0
|
下载量0
段落导航相关论文