| 注册
首页|期刊导航|理化检验-物理分册|自润滑关节轴承磨损失效分析

自润滑关节轴承磨损失效分析

袁兆静 李如琰

理化检验-物理分册2018,Vol.54Issue(5):374-377,4.
理化检验-物理分册2018,Vol.54Issue(5):374-377,4.DOI:10.11973/lhjy-wl201805016

自润滑关节轴承磨损失效分析

Failure Analysis on Wear of Self-Lubricating Spherical Plain Bearings

袁兆静 1李如琰1

作者信息

  • 1. 上海市轴承技术研究所,上海201801
  • 折叠

摘要

Abstract

The ceramic coating fracture phenonema appeared at the inner ring spherical surface of a self-lubricating spherical plain bearing used for a machine after using for 390 h.By means of macroscopic analysis, chemical composition analysis,scanning electron microscope and energy spectrum analysis and so on,the wear reasons of the bearing was analyzed.The results show that the self-lubricating spherical plain bearing had greater stress on one side,serious wear on this side of the bearing and concentrated force,which had exceeded the normal working condition,led to rapid wear and tear of ceramic coating at the inner ring spherical surface and liner in inner spheral surface of outer ring.In addition,the adhesion between ceramic coating near the end of the bearing and substrate was weak and easy to peeling,which can also led to wear and tear failure of the bearing.

关键词

自润滑关节轴承/陶瓷涂层/磨损/失效分析

Key words

self-lubricating spherical plain bearing/ceramic coating/wear/failure analysis

分类

机械制造

引用本文复制引用

袁兆静,李如琰..自润滑关节轴承磨损失效分析[J].理化检验-物理分册,2018,54(5):374-377,4.