Effects of annealing at different temperatures on microstructure and properties of Ti-3873 alloy welded joints

华允琪 1孙世博 1田宇航 1李壮 1吕坤琪 1张利1

作者信息

  • 1. 沈阳航空航天大学材料科学与工程学院 辽宁沈阳 110136
  • 折叠

摘要

Abstract

Microstructure and properties of Ti-3873 alloy laser welded joints after annealed at 450℃,550℃,650℃,750℃,respectively were studied.The experimental results show that the twins are observed in the HAZ of Ti-3873 alloy laser welded joints.The strength and hardness elevate and then drop with annealing temperatures increasing.The tensile strength reaches the maximal value of 1279.27MPa after annealing at 550℃.The annealing at 650℃of Ti-3873 alloy welded joints is the optimal process.

关键词

Ti-3873合金/热影响区/退火/孪晶/抗拉强度

Key words

Ti-3873 alloy/HAZ/annealing/twins/tensile strength

引用本文复制引用

华允琪,孙世博,田宇航,李壮,吕坤琪,张利..不同退火温度对Ti-3873合金焊接接头组织与性能的影响[J].金属加工(热加工),2024,(1):65-67,3.

基金项目

国家高技术研究发展计划(2015AA03A501) (2015AA03A501)

沈阳航空航天大学大学生创新创业训练计划(X202210143164). (X202210143164)

金属加工(热加工)

OACSTPCD

1674-165X

访问量0
|
下载量0
段落导航相关论文