Experimental Study on Stepwise Purification of Graphite Flotation Concentrates in Tanzania
坦桑尼亚石墨矿杂质多赋存于云母矿相中,依赖单一的氢氟酸未能有效除杂.本文以坦桑尼亚某已经球形化的石墨浮选精矿作为原料,通过氢氟酸/盐酸、硝酸/盐酸分步提纯的方法脱除杂质.氢氟酸浸出阶段,浸出时间为 5 h,温度为 50℃,氢氟酸用量为 24%,盐酸浓度为 25%,硝酸/盐酸浸出阶段,盐酸用量为 30%,硝酸用量为 20%,获得固定碳含量为 99.98%的高纯石墨,杂质金属含量低,满足电池负极材料的生产要求.本研究为坦桑尼亚石墨矿的深加工和开发应用提供技术支持.
The impurities of graphite ores in Tanzania are mostly present in the mica phase,and relying solely on hydrofluoric acid cannot effectively remove impurities.By using a spheroidized graphite flotation concentrate from Tanzania as raw material,this paper uses a stepwise purification method of hydrofluoric acid/hydrochloric acid and nitric acid/hydrochloric acid to remove impurities.In the hydrofluoric acid leaching stage,the leaching time is 5 h,the temperature is 50℃,the amount of hydrofluoric acid is 24%,and the concentration of hydrochloric acid is 25%,in the nitric acid/hydrochloric acid leaching stage,the amount of hydrochloric acid is 30%,and the amount of nitric acid is 20%,and high purity graphite with a fixed carbon content of 99.98%is obtained,and the impurity metal content is low,which meets the production requirements of battery negative electrode materials.This study provides technical support for the deep processing and development application of graphite ore in Tanzania.
冯嘉颖;刘建国;于丽丽;吕先谨;周吉奎
广东省科学院资源利用与稀土开发研究所||稀有金属分离与综合利用国家重点实验室,广州 510650广东省科学院资源利用与稀土开发研究所||稀有金属分离与综合利用国家重点实验室,广州 510650||昆明理工大学国土资源工程学院,昆明 650093广东省科学院资源利用与稀土开发研究所||稀有金属分离与综合利用国家重点实验室,广州 510650广东省科学院资源利用与稀土开发研究所||稀有金属分离与综合利用国家重点实验室,广州 510650广东省科学院资源利用与稀土开发研究所||稀有金属分离与综合利用国家重点实验室,广州 510650
化学工程
石墨浮选精矿分步提纯高纯石墨坦桑尼亚
graphite flotation concentratestepwise purificationhigh purity graphiteTanzania
《中国资源综合利用》 2023 (12)
1-4,4
广东省科学院专项资金项目(2022GDASZH-20220101042023GDASZH-2023010104).
评论