| 注册
首页|期刊导航|中国地质|西宁地区地热水环境中钢材腐蚀性能及防腐措施建议

西宁地区地热水环境中钢材腐蚀性能及防腐措施建议

赵振 秦光雄 耿松鹤 陈惠娟 晁嘉豪 张亮

中国地质2023,Vol.50Issue(6):1678-1690,13.
中国地质2023,Vol.50Issue(6):1678-1690,13.DOI:10.12029/gc20210503001

西宁地区地热水环境中钢材腐蚀性能及防腐措施建议

Corrosion performance of steel in geothermal water environment in Xining area and suggestions for anti-corrosion measures

赵振 1秦光雄 2耿松鹤 3陈惠娟 2晁嘉豪 3张亮3

作者信息

  • 1. 中国地质大学工程学院,湖北武汉 430074||青海省环境地质勘查局,青海西宁 810001||青海省环境地质重点实验室,青海西宁 810001||青海九零六工程勘察设计院有限责任公司,青海西宁 810001
  • 2. 青海省环境地质勘查局,青海西宁 810001||青海省环境地质重点实验室,青海西宁 810001||青海九零六工程勘察设计院有限责任公司,青海西宁 810001
  • 3. 中国石油大学(华东)石油工程学院,山东青岛 266580||中国石油大学(华东),非常规油气开发教育部重点实验室,山东青岛 266580
  • 折叠

摘要

Abstract

This paper is the result of geothermal survey engineering. [Objective]Xining area is rich in medium and low temperature geothermal resources,but the high salinity and strong corrosion of geothermal water limit the efficient development of geothermal energy.The proposed safe,economic and effective comprehensive well bucket anticorrosion measures are the basis and key to the effective utilization of high salinity geothermal resources.[Methods]In this study,the typical geothermal water in Xining area was collected,and the ionic composition and content of corrosive bacteria were tested.The high-temperature and high-pressure reactor was used to carry out metal plate corrosion tests to evaluate the corrosion performance of geothermal water on different steels under typical wellbore conditions.The corrosion type and the relationship between the corrosion rate and the influencing factors was analyzed.Finally,the anti-corrosion measures for geothermal water reinjection were proposed.[Results]The main corrosion components in geothermal water are Cl-,SO42-,H+ and dissolved oxygen,which cause uniform corrosion,platform corrosion and a small amount of pitting corrosion.The main corrosion products are FeO(OH)and Fe3O4;the corrosion rate along the wellbore gradually increases,and the corrosion risk at bottom hole is the greatest.In addition,the corrosion rate has a greater correlation with the geothermal water properties,P-T condition,flow speed and dissolved oxygen mixed into wellbore.[Conclusions]By fitting carbon steel corrosion experiment data,an empirical equation is established.The predicted value obtained by using the empirical equation is in good agreement with the experimental value.Safe,cost-effective and comprehensive wellbore anti-corrosion measures can be taken from the perspective of anti-corrosion pipes,reinjection geothermal water pretreatment,reinjection process parameters.

关键词

地热水回灌/挂片实验/腐蚀速率/氧气腐蚀/防腐措施/地热调查工程

Key words

geothermal water reinjection/metal plate test/corrosion rate/oxygen corrosion/anticorrosive measures/geothermal survey engineering

分类

天文与地球科学

引用本文复制引用

赵振,秦光雄,耿松鹤,陈惠娟,晁嘉豪,张亮..西宁地区地热水环境中钢材腐蚀性能及防腐措施建议[J].中国地质,2023,50(6):1678-1690,13.

基金项目

青海省应用基础研究计划项目(2020-ZJ-758)资助. Supported by Qinghai Applied Basic Research Project(No.2020-ZJ-758). (2020-ZJ-758)

中国地质

OA北大核心CSCDCSTPCD

1000-3657

访问量5
|
下载量0
段落导航相关论文