理化检验-物理分册2024,Vol.60Issue(6):56-58,3.DOI:10.11973/lhjy-wl230172
6061铝合金管材表面剥落原因
Causes of surface peel of aluminum 6061 alloy tube
杜艳华 1蔡振方 1董青1
作者信息
- 1. 中核新型材料研究与应用开发重点实验室,包头 014035||中核北方核燃料元件有限公司,包头 014035
- 折叠
摘要
Abstract
The surface peel of 6061 aluminum alloy tube occurred during turning.The surface peel area of aluminum alloy tube was studied by means of chemical composition analysis,scanning electron microscopy and energy spectrum analysis,and X-ray diffraction analysis.The results showed that there were a small amount of Al2O3,a small amount of SiO2,MgO and other oxide inclusions and a small amount of refining agent residues in the surface peel area.This was because in the process of aluminum alloy smelting,the removal of impurity elements and inclusions was not sufficient,and the aggregation of inclusions such as Al2O3 existed at the peel area.The hardness of Al2O3 inclusions was higher than that of aluminum matrix,resulting in peeling phenomenon.关键词
夹杂物/表面剥落/氧元素/X射线衍射/疏松Key words
inclusion/surface peel/oxygen element/X-ray diffraction/loose分类
矿业与冶金引用本文复制引用
杜艳华,蔡振方,董青..6061铝合金管材表面剥落原因[J].理化检验-物理分册,2024,60(6):56-58,3.