| 注册
首页|期刊导航|化工进展|原油组分及蜡晶结构对JH页岩油结构破坏与恢复的影响规律

原油组分及蜡晶结构对JH页岩油结构破坏与恢复的影响规律

尹然 穆野 霍富永 曹钦亮 蔺港归 王毅杰 黄启玉

化工进展2024,Vol.43Issue(z1):590-596,7.
化工进展2024,Vol.43Issue(z1):590-596,7.DOI:10.16085/j.issn.1000-6613.2024-0723

原油组分及蜡晶结构对JH页岩油结构破坏与恢复的影响规律

Influence of crude oil composition and wax crystal structure on the damage and recovery of JH shale oil structure

尹然 1穆野 2霍富永 1曹钦亮 3蔺港归 1王毅杰 2黄启玉2

作者信息

  • 1. 长庆工程设计有限公司,陕西西安 710005
  • 2. 中国石油大学(北京)机械与储运工程学院,油气管道输送安全国家工程实验室,城市油气输配技术北京市重点实验室,北京 102249
  • 3. 中国石油天然气股份有限公司长庆油田分公司新能源项目部,陕西西安 710005
  • 折叠

摘要

Abstract

The current energy development strategy of developing simultaneously oil and gas,as well as conventional and unconventional energy sources,effectively promotes the development process of shale oil,and the attention to its efficient and safe gathering and transportation process technology has been significantly increased.In this paper,the basic physical properties of JH shale oil were determined by indoor experiments,and its characteristics of low freezing point,low density,high wax content,high number of light components,no asphaltene,few colloids and weak wax crystal structure were identified.The wax crystal structure is easy to be destroyed during the gathering and transportation process,which will lead to the rapid decrease of dynamic viscosity near the freezing point.When the temperature of oil gathering is lower than the freezing point,the dynamic yield stress is significantly lower than the static value after stopping the transportation.After stopping the transportation,more wax crystals are precipitated during the static cooling process,which leads to the rapid recovery of condensate structural strength;under the condition of no temperature drop,the structural strength recovery is very slow,and the dynamic yield stress obtained after stopping the transportation for 12h at 9 ℃ below the freezing point is only 8.5%of the static value.In order to ensure the transportation safety,it is necessary to avoid the restart operation under the condition of low ground temperature or large temperature drop after stopping the transportation,and if necessary,intermittent startup can be used to reduce the yield stress of condensate,so as to ensure the restart safety.

关键词

含蜡页岩油/基础物性/流变特性/黏度/屈服应力/流动安全

Key words

waxy shale oil/basic physical properties/rheological properties/viscosity/yield stress/flow safety

分类

能源科技

引用本文复制引用

尹然,穆野,霍富永,曹钦亮,蔺港归,王毅杰,黄启玉..原油组分及蜡晶结构对JH页岩油结构破坏与恢复的影响规律[J].化工进展,2024,43(z1):590-596,7.

基金项目

国家自然科学基金重点项目(51534007) (51534007)

国家自然科学基金面上项目(51374224). (51374224)