长输管道外防腐技术应用及存在的问题

Application and Existing Problems of External Anti-corrosion Technology for Long-distance Pipeline

张本革 1张小燕 2吴天斌 3史乾坤1

作者信息

  • 1. 国家管网集团工程技术创新有限公司,天津 300450
  • 2. 中国石油天然气管道工程有限公司,河北 廊坊 065000
  • 3. 中国科学院化学研究所胶体、界面与化学热力学重点实验室,北京 100190
  • 折叠

摘要

Abstract

In order to improve the performance of the anti-corrosion coatings of long distance pipeline and meet the practical needs of pipeline engineering,the development status of the anti-corrosion technology of China's long distance oil and gas pipeline was analyzed,the advantages and disadvantages of various anti-corrosion coating properties were summarized,and the application of anti-corrosion technology of long distance pipeline was combined.The reasons for the high cost,high requirements of coating technology,difficulty of patching and easy mechanical damage of 3PE anti-corrosion coating and heat-bending pipe anti-corrosion coating,which are widely used at present,are analyzed,and the research direction of external anti-corrosion technology of long-haul pipeline is put forward.

关键词

长输管道/防腐/热煨弯管/机械化补口/3PE

Key words

long-distance pipeline/anti-corrosion/hot bending pipe/mechanized field patching/3PE