热处理对NEDDP/PBT并列复合长丝性能的影响

王凤霖 张艳茹 陈敏 姜爱娟 代国亮 王妮

纺织科学与工程学报2025,Vol.42Issue(2):22-28,34,8.
纺织科学与工程学报2025,Vol.42Issue(2):22-28,34,8.DOI:10.3969/j.issn.2096-5184.2025.02.004

热处理对NEDDP/PBT并列复合长丝性能的影响

The Effects of Heat Treatment on the Performance of NEDDP/PBT Parallel Composite Filament

王凤霖 1张艳茹 1陈敏 2姜爱娟 2代国亮 3王妮1

作者信息

  • 1. 东华大学产业用纺织品教育部工程研究中心,上海 201620||东华大学纺织学院,上海 201620
  • 2. 江苏箭鹿毛纺股份有限公司,安徽 宿迁 223800
  • 3. 军事科学院系统工程研究院军需工程技术研究所,北京 100082
  • 折叠

摘要

Abstract

In order to study the effects of heat treatment temperature,time and medium on the NEDDP/PBT parallel composite filament,the curling properties,mechanical properties and elastic properties of the NEDDP/PBT parallel composite filament were tested by using a fiber curling elasticity instrument and an XN-1A nylon e-longation and elasticity tester.The results show that as the heat treatment time increases and the temperature ri-ses,the curling rate,curling recovery rate,and curling elasticity rate of the NEDDP/PBT parallel composite fila-ment will increase and stabilize.Other conditions being the same,the filament with wet heat treatment has better curling rate,curling recovery rate and curling elasticity rate than the filament with dry heat treatment.As the heat treatment time increases and the temperature rises,the elongation at break of the filament increases and the breaking strength decreases.The elongation at break of the filament increases from 40.77%to 99.52%,and the breaking strength decreases from 137.63 cN to 116.37 cN.Other conditions being the same,the filament with wet heat treatment has a larger elongation at break and a smaller breaking strength than the filament with dry heat treatment.As the heat treatment time increases and the temperature rises,the elastic recovery rate and plas-tic deformation rate of the filament increase slightly.The elastic recovery rate is around 91.5%and the plastic deformation rate is around 3%.Other conditions being the same,the elastic recovery rate of the filament with wet heat treatment is similar to that of the filament with dry heat treatment,but the plastic deformation rate of the filament with wet heat treatment is slightly larger.

关键词

并列复合长丝/弹性/卷曲性/拉伸断裂性能

Key words

parallel composite filament/elasticity/curling property/tensile breaking properties