| 注册
首页|期刊导航|河南水利与南水北调|温湿度及养护材料对水工混凝土抗裂性能的影响分析

温湿度及养护材料对水工混凝土抗裂性能的影响分析

林秀彦

河南水利与南水北调2025,Vol.54Issue(2):48-50,3.
河南水利与南水北调2025,Vol.54Issue(2):48-50,3.

温湿度及养护材料对水工混凝土抗裂性能的影响分析

Analysis of Influence of Temperature and Humidity and Curing Materials on Crack Resistance of Hydraulic Concrete

林秀彦1

作者信息

  • 1. 山东省水利工程局有限公司,山东 济南 250013
  • 折叠

摘要

Abstract

The effect of different constant temperature and humidity conditions on the drying shrinkage of concrete are analyzed,and the improvement of crack resistance of concrete with different curing materials and different content under the condition of large temperature difference are explored.The results show that high temperature and high humidity will promote the internal water loss and intensify the drying shrinkage of concrete.In order to ensure the stability of concrete structure,appropriate temperature and humidity conditions should be maintained in engineering construction.Adding SAP and diatomite into concrete can promote the hydration reaction of cement,improve the compactness of concrete,and thus improve the compressive strength and splitting tensile strength of concrete.

关键词

水工混凝土/干燥收缩/养护材料/抗裂性能

Key words

hydraulic concrete/dry shrinkage/curing materials/crack resistance

分类

水利科学

引用本文复制引用

林秀彦..温湿度及养护材料对水工混凝土抗裂性能的影响分析[J].河南水利与南水北调,2025,54(2):48-50,3.

河南水利与南水北调

1673-8853

访问量0
|
下载量0
段落导航相关论文