脉冲激光工艺参数对M170P/DC06差厚拼焊接头组织与性能的影响

吴兴欢 赖春明 李乐攀

金属加工(热加工)Issue(9):48-54,62,8.
金属加工(热加工)Issue(9):48-54,62,8.

脉冲激光工艺参数对M170P/DC06差厚拼焊接头组织与性能的影响

Effect of pulse laser process parameters on microstructure and properties of M170P/DC06 differential thickness welded joints

吴兴欢 1赖春明 1李乐攀2

作者信息

  • 1. 湖南化工职业技术学院 湖南株洲 412000
  • 2. 湖南有色郴州氟化学有限公司 湖南郴州 423400
  • 折叠

摘要

Abstract

This study investigates the effects of pulse frequency,width,and voltage on the microstructure and mechanical properties of M170P/DC06 steel differential thickness plates welded joints using an SW-500 Nd:YAG pulsed laser.Results indicate that the DC06 steel thin plate HAZ exhibits coarse blocky ferrite,while the M170P steel thick plate HAZ consists of fine ferrite and granular bainite.Optimal hardness(200HV)is achieved at 20Hz pulse frequency and 300 mm/min welding speed,with a gradient decrease from thick to thin plate.

关键词

脉冲激光/差厚板/拼焊接头/显微组织

Key words

pulse laser/differential thickness plate/welding joints/microstructure

引用本文复制引用

吴兴欢,赖春明,李乐攀..脉冲激光工艺参数对M170P/DC06差厚拼焊接头组织与性能的影响[J].金属加工(热加工),2025,(9):48-54,62,8.