To address the issues of large in-process quantities and strict pot-life demands of slurry in traditional one-pot propellant slurry mixing,a static mixer mixing technique was designed and developed.In this technique,the pre-prepared binder slurry and curing agent slurry are stored separately in reservoirs,metered by screw pumps,extruded into a static mixer for blending,and then directly cast.Computational Fluid Dynamics(CFD)simulations were used to generate cloud images of the mixing pro-cess of a two-component slurry in a static mixer under typical conditions.A two-component curing system suitable for the static mixer mixing process was designed and synthesized.Based on this curing system,using K2SO4 and CaCO3 as simulated oxidiz-ers,a simulated oxidizer propellant with a solid content of 85%and without the addition of a bonding agent was prepared via the static mixer mixing process.The mechanical properties and microstructure of the propellant were characterized.Results indi-cate that the static mixer achieved homogeneous mixing of the two-component slurry.The resulting propellant exhibited a tensile strength of 0.4 MPa and an elongation at break of 37.5%,with a fracture surface that was dense and uniform,showing no cracks or voids.The static mixer mixing process offers advantages of small in-process quantity and no requirement for pot life of the slurry.

关键词

复合固体推进剂/混合工艺/静态混合器/端羟基聚丁二烯

Key words

composite solid propellant/mixing process/static mixer/hydroxyl-terminated polybutadiene