中国铸造2026,Vol.23Issue(1):83-93,11.DOI:10.1007/s41230-025-4083-4
Effect of cooling rate on solidification behavior and micro-segregation of high-alloyed wrought superalloy GH4975
Effect of cooling rate on solidification behavior and micro-segregation of high-alloyed wrought superalloy GH4975
摘要
关键词
Ni-based superalloy/cooling rate/solidification segregation/MC carbides/eutectic(γ+γ′)Key words
Ni-based superalloy/cooling rate/solidification segregation/MC carbides/eutectic(γ+γ′)分类
矿业与冶金引用本文复制引用
Guang-di Zhao,Xi-min Zang,Yi-xuan Sun,Xiao-yu Yao..Effect of cooling rate on solidification behavior and micro-segregation of high-alloyed wrought superalloy GH4975[J].中国铸造,2026,23(1):83-93,11.基金项目
This work was financially supported by the National Natural Science Foundation of China(Grant Nos.52474362,52174317 and 51904146)and the General Project Funded by Liaoning Province Education Department(Grant No.JYTMS20230943). (Grant Nos.52474362,52174317 and 51904146)