先进陶瓷(英文版)2025,Vol.14Issue(11):25-43,19.DOI:10.26599/JAC.2025.9221173
Construction of a molten CMAS-resistant bilayer-structured apatite layer used for thermal barrier coatings
Construction of a molten CMAS-resistant bilayer-structured apatite layer used for thermal barrier coatings
摘要
关键词
thermal barrier coatings(TBCs)/calcium-magnesium-alumina-silicate(CMAS)resistance/GdPO4/bilayer-structured apatite layer/CMAS wettingKey words
thermal barrier coatings(TBCs)/calcium-magnesium-alumina-silicate(CMAS)resistance/GdPO4/bilayer-structured apatite layer/CMAS wetting引用本文复制引用
Lanxin Zou,Yuxian Cheng,Shijun Meng,Lei Guo..Construction of a molten CMAS-resistant bilayer-structured apatite layer used for thermal barrier coatings[J].先进陶瓷(英文版),2025,14(11):25-43,19.基金项目
This research is sponsored by the Innovation Project(No.D925BCD),the National Natural Science Foundation of China(Nos.52471087 and 52272070),and the National Science and Technology Major Project(No.J2022-VI0009-0040). (No.D925BCD)