| 注册
首页|期刊导航|钢管|热轧无缝钢管外表面青线的产生与控制研究

热轧无缝钢管外表面青线的产生与控制研究

孙盼文 徐福昌 瞿海霞

钢管2026,Vol.55Issue(1):49-52,4.
✕
钢管2026,Vol.55Issue(1):49-52,4.DOI:10.19938/j.steelpipe.1001-2311.2026.1.49.52

热轧无缝钢管外表面青线的产生与控制研究

Research for the Formation and Control of Outer Surface Roll Trace on Hot-rolled Seamless Steel Pipe

孙盼文 1徐福昌 2瞿海霞1

作者信息

  • 1. 宝山钢铁股份有限公司,上海 201900
  • 2. 烟台鲁宝钢管有限责任公司,山东 烟台 265500
  • 折叠

摘要

Abstract

Addressing the outer surface roll trace defect of the hot-rolled seamless steel pipe,the causes are identi-fied by means of analyzing the key factors in the stretch reducing process as may lead to occurrence of the said defect,including roll quality,mill stand assembly,and pass configuration etc.Accordingly relevant countermeasures are worked out.It is revealed via the analysis that the surface roll trace primarily is caused by abnormal deformation of the tube at the stretch reducing roll surface or in the roll gap.Furthermore,inadequate roll performance or improper pass configuration can induce abnormal roll wear and crack,which also contribute to the formation of the surface roll trace.So it is suggested to effectively prevent the occurrence of the said defect via improvements associated with such aspects as stretch reducing roll quality,mill stand assembly accuracy,alignment precision of the rolling center line,and the pass configuration.

关键词

无缝钢管/青线/张力减径/轧辊/孔型

Key words

seamless steel pipe/surface roll trace/stretch reducing/roll/pass

引用本文复制引用

孙盼文,徐福昌,瞿海霞..热轧无缝钢管外表面青线的产生与控制研究[J].钢管,2026,55(1):49-52,4.