摘要

Abstract

A crack defect appeared on the connecting pipe of the liquid level gauge of the coal-to-methanol washing tower and the inner wall of the shell below it in a certain coal chemical factory.The reasons for the cracking of the connecting pipe were analyzed using macroscopic observation,penetration testing,chemical composition analysis,metallographic examination,scanning electron microscopy and energy dispersive spectroscopy analysis,mechanical property testing.The results show that during the operation of the washing tower,the entry of circulating water caused a decrease in temperature at the bottom of the connecting pipe and the inner wall of the shell below the connecting pipe.When the water supply was stopped,the temperature of the connecting pipe and the shell rose,causing cyclic thermal stress on the connecting pipe,ultimately leading to multi-source thermal fatigue cracking of the connecting pipe.

关键词

煤制甲醇洗涤塔/接管/多源热疲劳开裂/显微组织/热应力

Key words

coal-to-methanol washing tower/connection pipe/multi-source thermal fatigue cracking/microstructure/thermal stress