| 注册
首页|期刊导航|高校地质学报|地质聚合物原位封堵AMD的反应—固化协同机制研究

地质聚合物原位封堵AMD的反应—固化协同机制研究

刘迎澳 茅恒旗 叶涛 周来 亓增刚 吴剑锋 张凯凯

高校地质学报2026,Vol.32Issue(4):522-533,12.
✕
高校地质学报2026,Vol.32Issue(4):522-533,12.DOI:10.16108/j.issn1006-7493.2025047

地质聚合物原位封堵AMD的反应—固化协同机制研究

Study on the Reaction-Curing Synergistic Mechanism of Geopolymer in-situ Sealing of AMD

刘迎澳 1茅恒旗 1叶涛 1周来 1亓增刚 2吴剑锋 3张凯凯1

作者信息

  • 1. 矿山生态修复教育部工程研究中心,徐州 221116||中国矿业大学 环境与测绘学院,徐州 221116
  • 2. 中国煤炭地质总局物测队,邢台 054000||河北省煤炭地球物理勘探技术创新中心,邢台 054000
  • 3. 南京大学 地球科学与工程学院,南京 210023
  • 折叠

摘要

Abstract

In-situ injection of reactivity geopolymers can effectively seal Acid Mine Drainage(AMD),achieving the goals of source control and quality improvement of AMD.The reactivity and solidification performance of the grouting material are key parameters for the in-situ sealing of AMD using reactive geopolymers.This study aims to elucidate the synergistic mechanisms of the reactive geopolymers in AMD sealing and conducted experiments including grouting the material curing stability tests,dynamic AMD sealing experiments,and microscopic mechanism characterization.The results indicate that the grouting material exhibits good chemical stability and durability,with heavy metal leaching levels meeting national standards;the erosive effect of AMD can promote the formation of silicate and silicoaluminate substances,then effectively enhance the compressive strength of the nodule body to 6.37 MPa;under dynamic water conditions in an AMD environment,the dynamic blocking rate exceeded 90%.After grouting and blocking reactions,the final effluent pH increased from 3.6 to a range of 6.8 to 8.3.The removal rates of total Fe,Mn,and SO42-were above 98.8%,52.1%,and 33.3%,respectively.The increase in C-(A)-S-H and N-A-S-H gel products enhanced the ability of the solidified grouting body to solidify and stabilize heavy metals,while SO42-was converted into more sulfur-containing minerals;The geopolymer was used as a grouting agent injected into aquifers or filling zones,and the cement hydration,the generation of geopolymer,and the formation of the cement polymer were enhanced.hydration,the generation of geopolymer and the formation of hydrophobic film three reaction processes at the same time,under the erosion of acidic mine water,to promote the solidified body surface and the internal C-(A)-S-H,N-A-S-H gel products and Ca6Al2(SO4)3(OH)12(H2O)7,FeS,CaSO4 and other minerals,and at the same time,curing the heavy metals,formation of colloidal precipitates containing CaCO3,H2SiO3,Fe(OH)3,and Mn(OH)2 to meet the needs of green grouting.The synergistic mechanism of"grouting-reacting-solidifying-reducing"of the geopolymer grouting materials was clarified,which provides a scientific basis and practical guidance for the in-situ green management of AMD.

关键词

原位治理/反应性地质聚合物/酸性矿井水/注浆材料/协同机制

Key words

in-situ treatment/reactive geopolymer/acid mine drainage(amd)/grouting material/synergistic mechanism

分类

能源科技

引用本文复制引用

刘迎澳,茅恒旗,叶涛,周来,亓增刚,吴剑锋,张凯凯..地质聚合物原位封堵AMD的反应—固化协同机制研究[J].高校地质学报,2026,32(4):522-533,12.

基金项目

高硫矿区酸性地下水污染原位协同治理与防控体系:国家重点研发计划项目(2022YFC3702203)资助 (2022YFC3702203)